Between my research and experiments, the only thing I believe will stand up to very hot water is epoxy, or nothing. Kuksas are traditionally boiled in salt water and no finish is used. When I get back around to this again, that’s the way I will go next. But you’re probably ahead to use a stainless liner as suggested by OSU55.